API-571 Exam Question 46

Low creep ductility is __________ severe in high tensile strength materials and welds.
  • API-571 Exam Question 47

    Surface initiated cracks caused by environmental cracking of 300 Series SS and some nickel based alloys under the combined action of tensile stress, temperature and an aqueous chloride environmental is called ________. The presence of dissolved oxygen ___________ the propensity for cracking.
  • API-571 Exam Question 48

    The best way to prevent 885º F embrittlement is to use low ________ alloys, or to avoid exposing the susceptible material to the embrittling range.
  • API-571 Exam Question 49

    With sulfuric acid corrosion, the presence of oxidizers can _______ the corrosion rate.
  • API-571 Exam Question 50

    Naphthenic acid is _____ by catalytic reactions in downstream hydro processing and FCC units.