API-571 Exam Question 96

Type 304L SS is satisfactory for phosphoric acid concentration of 100% up to about _________. Type 321 is required from there to 225º F.
  • API-571 Exam Question 97

    MIC is often characterized by _______ within pits in carbon steel.
  • API-571 Exam Question 98

    ____________ is the reduction in toughness due to a metallurgical change that can occur in some low alloy steels as a result of long-term exposure in the temperature range of about 650º F to 1100º F.
  • API-571 Exam Question 99

    Carbonate stress corrosion cracking is the term applied to surface breaking or cracks that occur adjacent to carbon steel welds under the combined action of ____________ and ___________ in carbonate containing systems.
  • API-571 Exam Question 100

    In order to minimize and prevent amine SCC, PWHT all carbon steel welds in accordance with API RP _____.