API-571 Exam Question 106

Cavitation is best prevented by avoiding conditions that allow the absolute pressure to fall below the ___________ of the liquid or by changing the material properties.
  • API-571 Exam Question 107

    SSC is a form of ________ stress corrosion cracking.
  • API-571 Exam Question 108

    Areas of vulnerability in sulfuric acid Alkylation units include reactor effluent lines, reboilers, deisobutanizer, overhead systems and the _________ treating system.
  • API-571 Exam Question 109

    Preventative measures to minimize the potential for brittle fracture in existing equipment are limited to controlling _______ and ________, minimizing pressure at ambient temperatures during start-up and shutdown and periodic inspections at high stress locations.
  • API-571 Exam Question 110

    Ferritic stainless steels are usually not used in __________ applications.